Effect of Firing Temperature and Duration on Fused Silica Investment Shell Strength at Room Temperature

Research output: Contribution to journalArticlepeer-review

8 Scopus citations

Abstract

Fused silica is widely used in investment casting shell molds as flour, stucco and binder for its superior properties, such as low linear thermal expansion coefficient and high thermal shock resistance. Investment shell molds are usually fired after the de-wax process to remove the residue pattern material, and to improve shell strength through sintering. The firing temperatures are generally high enough to affect the phase constituent and microstructure of the shells, which further influences the shell strength. Firing duration at firing temperature is another important factor having an impact on the shell strength due to grain coarsening, but it is often overlooked by investment foundries. In this article, the room temperature moduli of rupture of investment shells fired at different conditions were determined. The crystallinity of fused silica shells was determined using X-ray diffraction. The differences on the shell strength were discussed and correlated with the microstructure and phase constitution in the shells after different firing processes.

Original languageEnglish
Pages (from-to)923-927
Number of pages5
JournalInternational Journal of Metalcasting
Volume13
Issue number4
DOIs
StatePublished - Oct 1 2019

Scopus Subject Areas

  • Mechanics of Materials
  • Metals and Alloys
  • Materials Chemistry
  • Industrial and Manufacturing Engineering

Keywords

  • firing duration
  • firing temperature
  • investment shell
  • modulus of rupture
  • phase transformation

Fingerprint

Dive into the research topics of 'Effect of Firing Temperature and Duration on Fused Silica Investment Shell Strength at Room Temperature'. Together they form a unique fingerprint.

Cite this